Hard ferrite powder for bonded magnets has a wide application,for example, isotropic magnetic ferrite powder can be used in manufacture of sound dampening of automotive, fridge magnets, visual ads and sealing strip. Injection molding magnetic powder used in manufacture of rigid motor magnets, magnetic roll of copier and printer, anisotropic calendaring magnetic ferrite powder used in manufacture of flexible motor magnets.

|
P/N |
Material |
Find Powder (µm) |
Moisture % |
Magnetic Properties |
Testing Mothed | |||
|
Br |
bHc |
iHc |
(BH)max | |||||
|
mT |
(kA/m) |
(kA/m) |
(KJ/m3) | |||||
|
BMXF-2D |
BaFe12O19 |
2.0±0.4 |
≤0.5 |
145±5 |
95±16 |
195±25 |
3.5±0.4 |
Green Piece |
|
BMXF-2SH |
SrFe12O19 |
1.7±0.3 |
≤0.5 |
145±5 |
95±16 |
195±12 |
3.5±0.4 |
Green Piece |
|
225±10 |
135±16 |
172±12 |
9.0±1.0 |
Calendering | ||||
|
BMXF-3D |
SrFe12O19 |
1.80±0.20 |
≤0.5 |
170±5 |
115±6 |
219±12 |
5.2±0.5 |
Green Piece |
|
290±5 |
203±12 |
235±16 |
15.9±0.8 |
Injection | ||||
|
BMXF-4D |
SrFe12O19 |
1.2±0.1 |
≤0.5 |
157±5 |
110±5 |
≥240 |
4.6±0.3 |
Green Piece |
|
264±6 |
185±5 |
240±15 |
13.0±0.8 |
Calendering | ||||
|
BMXF-4DH |
SrFe12O19 |
1.20±0.15 |
≤0.5 |
157±5 |
110±5 |
306±12 |
4.6±0.3 |
Green Piece |
|
262±5 |
185±5 |
345±25 |
13.0±0.8 |
Calendering | ||||
|
BMXF-4D2 |
SrFe12O19 |
1.2±0.1 |
≤0.5 |
160±5 |
110±5 |
252±12 |
4.7±0.3 |
Green Piece |
|
260±5 |
180±5 |
235±25 |
13.0±0.8 |
Calendering | ||||
|
BMXF-4D3 |
SrFe12O19 |
1.20±0.15 |
≤0.5 |
155±5 |
110±5 |
277±12 |
4.5±0.3 |
Green Piece |
|
257±5 |
183±5 |
257±25 |
12.8±0.8 |
Calendering | ||||